Product Detailed
1)Taking pet chip as raw materials
2)Processing method: biaxially oriented strengthing
3)Good tensile Strength
Specification:Usage:Advantages:
Testing Report (12 micro) |
Testing Item (Aluminizing level) | STANDARD | RESULTS |
Thickness(micron) | 12 | 11.98 |
Tensile Strength(Mpa) | MD | ≥200 | 228 |
TD | ≥200 | 217 |
Break Elongation (%) | MD | ≥100 | 119 |
TD | ≥100 | 147 |
Modulus of Elasticity (Mpa) | MD | ≥4000 | 4538 |
TD | ≥4000 | 4276 |
Heat Shrinkage %(150°C,30min) | MD | ≤2.0 | 1.3 |
TD | ≤0.2 | -0.21 |
Friction Factor | ≤0.6 | 0.472=4/0.530 |
Haze (%) | ≤3 | 2 |
Density (g/cm3) | 1.39-1.41 | 1.4 |
Transmittance (%) | ≥89 | 90 |
Glossiness (%) | ≥100 | 133 |
Surface Tension (dye) mN/m | ≥50 | 54 |